Polymer Property : CTE, linear = -6.00 µm/m-°C Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
CTE, linear -6.00 µm/m-°C

@Thickness 0.0508 mm
-3.33 µin/in-°F

@Thickness 0.00200 in
first heat; ASTM D 696
3M 468MP High Performance Adhesive Transfer Tapes with Adhesive 200MP
3M™ High Performance Acrylic Adhesive 200MP is a popular choice for graphic attachment and membrane switch applications because it has excellent quality, consistency and durability. In addition, as..
CTE, linear -6.00 µm/m-°C

@Thickness 0.0508 mm
-3.33 µin/in-°F

@Thickness 0.00200 in
first heat; ASTM D 696
3M 9667MP High Performance Adhesive Transfer Tapes with Adhesive 200MP
3M™ High Performance Acrylic Adhesive 200MP is a popular choice for graphic attachment and membrane switch applications because it has excellent quality, consistency and durability. In addition, as..
CTE, linear -6.00 µm/m-°C

@Thickness 0.0508 mm
-3.33 µin/in-°F

@Thickness 0.00200 in
first heat; ASTM D 696
3M 9668MP High Performance Adhesive Transfer Tapes with Adhesive 200MP
3M™ High Performance Acrylic Adhesive 200MP is a popular choice for graphic attachment and membrane switch applications because it has excellent quality, consistency and durability. In addition, as..
CTE, linear -6.00 µm/m-°C

@Thickness 0.0508 mm
-3.33 µin/in-°F

@Thickness 0.00200 in
first heat; ASTM D 696
3M 7952MP High Performance Adhesive Transfer Tapes with Adhesive 200MP
3M™ High Performance Acrylic Adhesive 200MP is a popular choice for graphic attachment and membrane switch applications because it has excellent quality, consistency and durability. In addition, as..
CTE, linear -6.00 µm/m-°C

@Thickness 0.0508 mm
-3.33 µin/in-°F

@Thickness 0.00200 in
first heat; ASTM D 696
3M 7962MP High Performance Adhesive Transfer Tapes with Adhesive 200MP
3M™ High Performance Acrylic Adhesive 200MP is a popular choice for graphic attachment and membrane switch applications because it has excellent quality, consistency and durability. In addition, as..
CTE, linear -6.00 µm/m-°C

@Thickness 0.0508 mm
-3.33 µin/in-°F

@Thickness 0.00200 in
first heat; ASTM D 696
3M 9172MP High Performance Adhesive Transfer Tapes with Adhesive 200MP
3M™ High Performance Acrylic Adhesive 200MP is a popular choice for graphic attachment and membrane switch applications because it has excellent quality, consistency and durability. In addition, as..
CTE, linear -6.00 µm/m-°C

@Thickness 0.0508 mm
-3.33 µin/in-°F

@Thickness 0.00200 in
first heat; ASTM D 696
3M 9185MP High Performance Adhesive Transfer Tapes with Adhesive 200MP
3M™ High Performance Acrylic Adhesive 200MP is a popular choice for graphic attachment and membrane switch applications because it has excellent quality, consistency and durability. In addition, as..
CTE, linear -6.00 µm/m-°C

@Thickness 0.0508 mm
-3.33 µin/in-°F

@Thickness 0.00200 in
first heat; ASTM D 696
3M 467MP High Performance Adhesive Transfer Tapes with Adhesive 200MP
3M™ High Performance Acrylic Adhesive 200MP is a popular choice for graphic attachment and membrane switch applications because it has excellent quality, consistency and durability. In addition, as..
CTE, linear -6.00 µm/m-°C

@Thickness 0.0508 mm
-3.33 µin/in-°F

@Thickness 0.00200 in
first heat; ASTM D 696
3M 467MPF High Performance Adhesive Transfer Tapes with Adhesive 200MP
3M™ High Performance Acrylic Adhesive 200MP is a popular choice for graphic attachment and membrane switch applications because it has excellent quality, consistency and durability. In addition, as..
CTE, linear -6.00 µm/m-°C

@Thickness 0.0508 mm
-3.33 µin/in-°F

@Thickness 0.00200 in
first heat; ASTM D 696
3M 468MPF High Performance Adhesive Transfer Tapes with Adhesive 200MP
3M™ High Performance Acrylic Adhesive 200MP is a popular choice for graphic attachment and membrane switch applications because it has excellent quality, consistency and durability. In addition, as..
CTE, linear -6.00 µm/m-°C

@Thickness 0.0508 mm
-3.33 µin/in-°F

@Thickness 0.00200 in
first heat; ASTM D 696
3M 7955MP High Performance Adhesive Transfer Tapes with Adhesive 200MP
3M™ High Performance Acrylic Adhesive 200MP is a popular choice for graphic attachment and membrane switch applications because it has excellent quality, consistency and durability. In addition, as..
CTE, linear -6.00 µm/m-°C

@Thickness 0.0508 mm
-3.33 µin/in-°F

@Thickness 0.00200 in
first heat; ASTM D 696
3M 7965MP High Performance Adhesive Transfer Tapes with Adhesive 200MP
3M™ High Performance Acrylic Adhesive 200MP is a popular choice for graphic attachment and membrane switch applications because it has excellent quality, consistency and durability. In addition, as..