Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear | 10.69 µm/m-°C @Temperature 500 °C |
5.939 µin/in-°F @Temperature 932 °F |
|
Mykroy/Mycalex MM 800 Machining Grade Glass-bonded Mica Composite MM 800 (formerly MM 1600) is a compression molded glass mica composite that is the perfect alternative to high performance plastics where high temperature, good dielectric strength and good arc resi.. |