Thermal Properties Metric English Comments
CTE, linear 11.02 µm/m-°C

@Temperature 24.0 - 427 °C
6.122 µin/in-°F

@Temperature 75.2 - 801 °F
QuesTek® Innovations Ferrium® S53® Corrosion Resistant High Strength Steel for Aerospace Structural Applications
Description: Ferrium® S53® is a corrosion resistant ultra high-strength steel for structural aerospace applications. Ferrium® S53® was designed to provide mechanical properties equal to, or bett..