Polymer Property : CTE, linear = 11.15 µm/m-°C Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
CTE, linear 11.15 µm/m-°C

@Temperature 21.0 - 204 °C
6.194 µin/in-°F

@Temperature 69.8 - 399 °F
Latrobe Graph-Mo® Cold Work Tool Steel (ASTM O6)
Graph-Mo tool steel is an oil-hardening, graphitic tool steel with outstanding resistance to metal-to-metal sliding wear and galling. The steel contains a uniform dispersion of graphite particles wh..