Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear | 11.25 µm/m-°C @Temperature 21.0 - 100 °C |
6.250 µin/in-°F @Temperature 69.8 - 212 °F |
|
Carpenter Micro-Melt® 9 Hardened and Tempered Tool Steel Micro-Melt® 9 tool steel is a high vanadium tool steel produced using the Carpenter Micro-Melt powder process. This grade possesses wear resistance superior to most other tool steels along with goo.. |
|||
CTE, linear | 11.25 µm/m-°C @Temperature 20.0 - 480 °C |
6.250 µin/in-°F @Temperature 68.0 - 896 °F |
|
ATI Allegheny Ludlum AL 433™ Ferritic Stainless Steel, Annealed AL 433™ is a stainless steel in the ferritic family of alloys with Type 409 and Type 439. The AL 433 alloy contains 20% chromium for pitting and crevice corrosion resistance in the presence of chl.. |