Polymer Property : CTE, linear = 11.68 µm/m-°C Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
CTE, linear 11.68 µm/m-°C

@Temperature 21.0 - 204 °C
6.489 µin/in-°F

@Temperature 69.8 - 399 °F
Latrobe Tatmo-VN™ ASTM M7 High Speed Steel