Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear | 11.8 µm/m-°C @Temperature 20.0 - 300 °C |
6.56 µin/in-°F @Temperature 68.0 - 572 °F |
|
International Mold Steel Daido DRM2 Matrix High-Speed Steel This matrix type high speed tool steel is available for warm and cold forging tools where critical performance is required. DRM2 prolongs service life due to its higher hardness and toughness than t.. |
|||
CTE, linear | 11.8 µm/m-°C @Temperature >=300 °C |
6.56 µin/in-°F @Temperature >=572 °F |
|
International Mold Steel DH21 Die Cast & Forging Steel DH21 is for aluminum die cast dies.Information provided by International Mold Steel |
|||
CTE, linear | 11.8 µm/m-°C @Temperature 20.0 - 300 °C |
6.56 µin/in-°F @Temperature 68.0 - 572 °F |
|
International Mold Steel DH31-EX Die Cast & Forging Steel DH31-EX is a hot working die steel with the best balance of strength and toughness showing the comparable softening resistance to SKD7 and twice hardenability as that of SKD61.Information provided b.. |
|||
CTE, linear | 11.8 µm/m-°C @Temperature 25.0 - 600 °C |
6.56 µin/in-°F @Temperature 77.0 - 1110 °F |
|
Haynes Hastelloy® B-3® alloy, 0% cold work The attributes of Corrosion-Resistant HASTELLOY® alloys include high resistance to uniform attack, outstanding localized corrosion resistance, excellent stress corrosion cracking resistance, and .. |
|||
CTE, linear | 11.8 µm/m-°C @Temperature 25.0 - 500 °C |
6.56 µin/in-°F @Temperature 77.0 - 932 °F |
|
Haynes Hastelloy® B-3® alloy, 0% cold work The attributes of Corrosion-Resistant HASTELLOY® alloys include high resistance to uniform attack, outstanding localized corrosion resistance, excellent stress corrosion cracking resistance, and .. |
|||
CTE, linear | 11.8 µm/m-°C @Temperature 25.0 - 600 °C |
6.56 µin/in-°F @Temperature 77.0 - 1110 °F |
|
Haynes Hastelloy® B-3® alloy, 10% cold work The attributes of Corrosion-Resistant HASTELLOY® alloys include high resistance to uniform attack, outstanding localized corrosion resistance, excellent stress corrosion cracking resistance, and .. |
|||
CTE, linear | 11.8 µm/m-°C @Temperature 25.0 - 500 °C |
6.56 µin/in-°F @Temperature 77.0 - 932 °F |
|
Haynes Hastelloy® B-3® alloy, 10% cold work The attributes of Corrosion-Resistant HASTELLOY® alloys include high resistance to uniform attack, outstanding localized corrosion resistance, excellent stress corrosion cracking resistance, and .. |
|||
CTE, linear | 11.8 µm/m-°C @Temperature 25.0 - 600 °C |
6.56 µin/in-°F @Temperature 77.0 - 1110 °F |
|
Haynes Hastelloy® B-3® alloy, 20% cold work The attributes of Corrosion-Resistant HASTELLOY® alloys include high resistance to uniform attack, outstanding localized corrosion resistance, excellent stress corrosion cracking resistance, and .. |
|||
CTE, linear | 11.8 µm/m-°C @Temperature 25.0 - 500 °C |
6.56 µin/in-°F @Temperature 77.0 - 932 °F |
|
Haynes Hastelloy® B-3® alloy, 20% cold work The attributes of Corrosion-Resistant HASTELLOY® alloys include high resistance to uniform attack, outstanding localized corrosion resistance, excellent stress corrosion cracking resistance, and .. |
|||
CTE, linear | 11.8 µm/m-°C @Temperature 25.0 - 600 °C |
6.56 µin/in-°F @Temperature 77.0 - 1110 °F |
|
Haynes Hastelloy® B-3® alloy, 3.2 mm bright annealed sheet The attributes of Corrosion-Resistant HASTELLOY® alloys include high resistance to uniform attack, outstanding localized corrosion resistance, excellent stress corrosion cracking resistance, and .. |
|||
CTE, linear | 11.8 µm/m-°C @Temperature 25.0 - 500 °C |
6.56 µin/in-°F @Temperature 77.0 - 932 °F |
|
Haynes Hastelloy® B-3® alloy, 3.2 mm bright annealed sheet The attributes of Corrosion-Resistant HASTELLOY® alloys include high resistance to uniform attack, outstanding localized corrosion resistance, excellent stress corrosion cracking resistance, and .. |
|||
CTE, linear | 11.8 µm/m-°C @Temperature 25.0 - 600 °C |
6.56 µin/in-°F @Temperature 77.0 - 1110 °F |
|
Haynes Hastelloy® B-3® alloy, 30% cold work The attributes of Corrosion-Resistant HASTELLOY® alloys include high resistance to uniform attack, outstanding localized corrosion resistance, excellent stress corrosion cracking resistance, and .. |
|||
CTE, linear | 11.8 µm/m-°C @Temperature 25.0 - 500 °C |
6.56 µin/in-°F @Temperature 77.0 - 932 °F |
|
Haynes Hastelloy® B-3® alloy, 30% cold work The attributes of Corrosion-Resistant HASTELLOY® alloys include high resistance to uniform attack, outstanding localized corrosion resistance, excellent stress corrosion cracking resistance, and .. |
|||
CTE, linear | 11.8 µm/m-°C @Temperature 25.0 - 600 °C |
6.56 µin/in-°F @Temperature 77.0 - 1110 °F |
|
Haynes Hastelloy® B-3® alloy, 40% cold work The attributes of Corrosion-Resistant HASTELLOY® alloys include high resistance to uniform attack, outstanding localized corrosion resistance, excellent stress corrosion cracking resistance, and .. |
|||
CTE, linear | 11.8 µm/m-°C @Temperature 25.0 - 500 °C |
6.56 µin/in-°F @Temperature 77.0 - 932 °F |
|
Haynes Hastelloy® B-3® alloy, 40% cold work The attributes of Corrosion-Resistant HASTELLOY® alloys include high resistance to uniform attack, outstanding localized corrosion resistance, excellent stress corrosion cracking resistance, and .. |
|||
CTE, linear | 11.8 µm/m-°C @Temperature 25.0 - 600 °C |
6.56 µin/in-°F @Temperature 77.0 - 1110 °F |
|
Haynes Hastelloy® B-3® alloy, 50% cold work The attributes of Corrosion-Resistant HASTELLOY® alloys include high resistance to uniform attack, outstanding localized corrosion resistance, excellent stress corrosion cracking resistance, and .. |
|||
CTE, linear | 11.8 µm/m-°C @Temperature 25.0 - 500 °C |
6.56 µin/in-°F @Temperature 77.0 - 932 °F |
|
Haynes Hastelloy® B-3® alloy, 50% cold work The attributes of Corrosion-Resistant HASTELLOY® alloys include high resistance to uniform attack, outstanding localized corrosion resistance, excellent stress corrosion cracking resistance, and .. |
|||
CTE, linear | 11.8 µm/m-°C @Temperature 25.0 - 600 °C |
6.56 µin/in-°F @Temperature 77.0 - 1110 °F |
|
Haynes Hastelloy® B-3® alloy, 6.3 mm plate The attributes of Corrosion-Resistant HASTELLOY® alloys include high resistance to uniform attack, outstanding localized corrosion resistance, excellent stress corrosion cracking resistance, and .. |
|||
CTE, linear | 11.8 µm/m-°C @Temperature 25.0 - 500 °C |
6.56 µin/in-°F @Temperature 77.0 - 932 °F |
|
Haynes Hastelloy® B-3® alloy, 6.3 mm plate The attributes of Corrosion-Resistant HASTELLOY® alloys include high resistance to uniform attack, outstanding localized corrosion resistance, excellent stress corrosion cracking resistance, and .. |
|||
CTE, linear | 11.8 µm/m-°C @Temperature 21.1 - 427 °C |
6.58 µin/in-°F @Temperature 70.0 - 800 °F |
|
Crucible Steel REX® M2 S 1.0C High Speed Steel, AISI M2 REX M2S (1.0C) is a sulfur-bearing high carbon version of the regular CRUCIBLE REX M2 high speed steel. The sulfur addition provides good grindability and an improvement in machinability of 25 to 35.. |
|||
CTE, linear | 11.8 µm/m-°C @Temperature 21.1 - 427 °C |
6.58 µin/in-°F @Temperature 70.0 - 800 °F |
|
Crucible Steel REX® M2 S High Speed Steel REX M2 is a tungsten-molybdenum high speed steel which gives outstanding performance in all operations where a general purpose high speed steel is required. REX M2 has a wide hardening range, excell.. |
|||
CTE, linear | 11.8 µm/m-°C @Temperature 20.0 - 427 °C |
6.56 µin/in-°F @Temperature 68.0 - 801 °F |
|
Bohler-Uddeholm BÖHLER K294 MICROCLEAN AISI A11 Powder Metal Tool Steel Properties: Powder-metallurgical produced cold work tool steel with extremely high wear resistance, good toughness and high compressive strength. The latest generation of powder metal technology ena.. |
|||
CTE, linear | 11.8 µm/m-°C @Temperature 20.0 - 199 °C |
6.55 µin/in-°F @Temperature 68.0 - 390 °F |
|
Bohler-Uddeholm BÖHLER K340 ISODUR® Premium Cold Work Steel BÖHLER K340 ISODUR is a universal cold work tool steel with which you‘ll be making money and just when blanking coins, but also when: blanking, cutting, cold rolling, extruding, deep drawing and b.. |
|||
CTE, linear | 11.8 µm/m-°C @Temperature 20.0 - 100 °C |
6.56 µin/in-°F @Temperature 68.0 - 212 °F |
|
Carpenter Vega® Alloy Tool Steel (Air-Tough) (AISI A6) Vega die steel combines the deep hardening and minimum size change characteristics of air-hardening steels with the simplicity of low temperature heat treatment possible in many oil-hardening steels.. |
|||
CTE, linear | 11.8 µm/m-°C @Temperature 20.0 - 400 °C |
6.56 µin/in-°F @Temperature 68.0 - 752 °F |
for the hardened and tempered condition |
Assab Steels ASP 30 Cold Work Steel ASP 30 is a W-Mo-v-Co alloyed PM high speed steel characterized by:High wear resistanceHigh compressive strength at high hardnessGood through hardening propertiesGood toughnessGood dimensional stabi.. |
|||
CTE, linear | 11.8 µm/m-°C @Temperature 25.0 - 600 °C |
6.56 µin/in-°F @Temperature 77.0 - 1110 °F |
|
Haynes Hastelloy® B-3® alloy, heat treated at 1065°C, rapid quenched The attributes of Corrosion-Resistant HASTELLOY® alloys include high resistance to uniform attack, outstanding localized corrosion resistance, excellent stress corrosion cracking resistance, and ea.. |
|||
CTE, linear | 11.8 µm/m-°C @Temperature 25.0 - 500 °C |
6.56 µin/in-°F @Temperature 77.0 - 932 °F |
|
Haynes Hastelloy® B-3® alloy, heat treated at 1065°C, rapid quenched The attributes of Corrosion-Resistant HASTELLOY® alloys include high resistance to uniform attack, outstanding localized corrosion resistance, excellent stress corrosion cracking resistance, and ea.. |