Polymer Property : CTE, linear = 111 µin/in-°F Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
CTE, linear 200 µm/m-°C

@Temperature 20.0 °C
111 µin/in-°F

@Temperature 68.0 °F
Cured property; alpha 2; Perkin Elmer TMS-2
Aptek 6108-PMF Epoxy Coating/Encapsulant
High temperature, rigid, electrical/electronic coating or encapsulant. Provides excellent environmental protection for continuous exposure to 220°C.Information provided by Aptek Laboratories, Inc.
CTE, linear 200 µm/m-°C

@Temperature 20.0 °C
111 µin/in-°F

@Temperature 68.0 °F
Cured property; alpha 2; Perkin Elmer TMS-2
Aptek 6108-PMF Epoxy Encapsulant and/or Potting Compound
High temperature, rigid, electrical/electronic coating or encapsulant. Provides excellent environmental protection for continuous exposure to 220°C. Also can be used as a high temperature wire varn..
CTE, linear 200 µm/m-°C

@Temperature -50.0 - 110 °C
111 µin/in-°F

@Temperature -58.0 - 230 °F
3M Scotch-Weld™ DP110 Translucent Epoxy Adhesive
3M™ Scotch-Weld™ Epoxy Adhesive DP110 Translucent and Gray are two-part epoxy adhesive which combine a fast cure with flexibilityInformation provided by 3M
CTE, linear 200 µm/m-°C

@Temperature >=55.0 °C
111 µin/in-°F

@Temperature >=131 °F
above Tg
Resinlab® EP1115 Clear Unfilled Epoxy Adhesive
Resinlab™ EP1115 Clear is a two part unfilled epoxy adhesive designed for bonding of metals, ceramics and most plastics. This product gives good resistance to water, salt spray, inorganic acids and..