Polymer Property : CTE, linear = 114.5 µm/m-°C Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
CTE, linear 106.5 - 114.5 µm/m-°C

@Temperature 0.000 - 50.0 °C
59.17 - 63.61 µin/in-°F

@Temperature 32.0 - 122 °F
ASTM E831-05
DSM Somos® NeXT Stereolithography (SLA) Prototyping Polymer
Somos® NeXT combines stiffness and impact resistance which brings it close the performance of injection molded thermoplastics. It produces finished parts with tight tolerances and detailed features..