Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear | 12.02 µm/m-°C @Temperature 38.0 - 538 °C |
6.678 µin/in-°F @Temperature 100 - 1000 °F |
|
Latrobe LSSâ„¢ D5 Tool Steel (ASTM D5) TLS D5 tool steel is an air hardening, high-carbon, high-chromium, tool steel that is characterized by a cobalt addition which provides unique resistance to galling and pick-up. The cobalt also impa.. |