Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear | 22.1 µm/m-°C @Temperature 20.0 °C |
12.3 µin/in-°F @Temperature 68.0 °F |
Across Surface; ASTM D-696 |
Glastic GLASTHERM HT200 Insulation Sheet HT200 features:High Hot Compressive StrengthLow Thermal ConductivityOil and Moisture ResistantReduces Heat LossHelps Control TemperatureFaster Mold StartupDesigned for reducing heat losses from plas.. |
|||
CTE, linear | 22.1 µm/m-°C @Temperature 20.0 °C |
12.3 µin/in-°F @Temperature 68.0 °F |
Across Surface; ASTM D-696 |
Glastic GLASTHERM HT Insulation Sheet Glastherm Grade HT is a high compressive strength, heat-resistant composite material. It is ideal for insulation between the fold and the press or within the mold itself. Grade HT is completely as.. |