Thermal Properties Metric English Comments
CTE, linear 12.38 µm/m-°C

@Temperature 100 °C
6.878 µin/in-°F

@Temperature 212 °F
Special Metals INCONEL® alloy 740 Precipitation-Hardenable Ni-Cr-Co Superalloy
INCONEL® alloy 740 is a nickel-chromium-cobalt alloy developed by Special Metals Corporation. The alloy is age hardenable by the precipitation of a gamma prime second phase. Potential applicati..