Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear | 12.5 µm/m-°C @Temperature 25.0 °C |
6.94 µin/in-°F @Temperature 77.0 °F |
|
Mykroy/Mycalex MM 400 Machining Grade Glass-bonded Mica Composite Natural mica filler. Does not burn. Good radiation resistance (3 x 10^10 Rads-Cobalt).This ceramoplastic material is a versatile and efficient insulating material designed to meet the exacting dem.. |
|||
CTE, linear | 12.5 µm/m-°C @Temperature 0.000 - 200 °C |
6.94 µin/in-°F @Temperature 32.0 - 392 °F |
|
Kennametal Stellite Stellite® 3 PM with P/M Processing Typical applications include (aerospace) vane plugs, fuel metering pins, spacer bushings, (bearings) ball blanks, race blanks, (valve seat inserts) diesel engine exhaust, fluid valve seats, saw cutt.. |
|||
CTE, linear | 12.5 µm/m-°C @Temperature 20.0 - 300 °C |
6.94 µin/in-°F @Temperature 68.0 - 572 °F |
|
Industeel CREUSABRO® 4000 High Wear Resistant Steel Description: CREUSABRO® 4000 is a high wear resistant steel, offering a 30 % extra in service life compared to a conventional 400 HB water quenched. Improved properties of CREUSABRO® 4000 resu.. |
|||
CTE, linear | 12.5 µm/m-°C @Temperature 25.0 - 400 °C |
6.94 µin/in-°F @Temperature 77.0 - 752 °F |
|
Haynes Hastelloy® Hybrid-BC1® Nickel Alloy Bar, Hot Rolled and Solution Annealed HASTELLOY® HYBRID-BC1® alloy possesses much higher resistance to hydrochloric and sulfuric acids than the nickel-chromium-molybdenum (C-type) alloys, and can tolerate the presence of oxidizing.. |
|||
CTE, linear | 12.5 µm/m-°C @Temperature 25.0 - 400 °C |
6.94 µin/in-°F @Temperature 77.0 - 752 °F |
|
Haynes Hastelloy® Hybrid-BC1® Nickel Alloy Shielded Metal Arc Welded (SMAW) Plate HASTELLOY® HYBRID-BC1® alloy possesses much higher resistance to hydrochloric and sulfuric acids than the nickel-chromium-molybdenum (C-type) alloys, and can tolerate the presence of oxidizing.. |
|||
CTE, linear | 12.5 µm/m-°C @Temperature 25.0 - 400 °C |
6.94 µin/in-°F @Temperature 77.0 - 752 °F |
|
Haynes Hastelloy® Hybrid-BC1® Nickel Alloy Gas Tungsten Arc Welded (GTAW) Plate HASTELLOY® HYBRID-BC1® alloy possesses much higher resistance to hydrochloric and sulfuric acids than the nickel-chromium-molybdenum (C-type) alloys, and can tolerate the presence of oxidizing.. |
|||
CTE, linear | 12.5 µm/m-°C @Temperature 25.0 - 400 °C |
6.94 µin/in-°F @Temperature 77.0 - 752 °F |
|
Haynes Hastelloy® Hybrid-BC1® Nickel Alloy Sheet, Cold Rolled and Solution Annealed HASTELLOY® HYBRID-BC1® alloy possesses much higher resistance to hydrochloric and sulfuric acids than the nickel-chromium-molybdenum (C-type) alloys, and can tolerate the presence of oxidizing.. |
|||
CTE, linear | 12.5 µm/m-°C @Temperature 20.0 - 540 °C |
6.94 µin/in-°F @Temperature 68.0 - 1000 °F |
|
Crucible Steel CPM® REX® 66 (HS) High Speed Steel CPM Rex 66 is a super high speed steel made by the Crucible Particle Metallurgy (CPM) process. It is a tungsten type high speed with a high vanadium content for excellent abrasion resistance, simila.. |
|||
CTE, linear | 12.5 µm/m-°C @Temperature 40.0 - 540 °C |
6.94 µin/in-°F @Temperature 104 - 1000 °F |
|
Crucible Steel Rex M2 High Speed Steel Rex M2 is a tungsten-molybdenum general purpose high speed steel. It is suitable for a wide variety of cutting tools and is often used for metalforming tools such as punches and dies. Rex M2 is a go.. |
|||
CTE, linear | 12.5 µm/m-°C @Temperature 37.8 - 538 °C |
6.93 µin/in-°F @Temperature 100 - 1000 °F |
|
Crucible Steel REX® TMO High Speed Steel, AISI M1 REX TMO molybdenum-tungsten high speed steel is a tough general purpose high speed steel with high cutting efficiency and excellent finishing properties. It is adapted to fast light cuts on soft or .. |
|||
CTE, linear | 12.5 µm/m-°C @Temperature 700 °C |
6.94 µin/in-°F @Temperature 1290 °F |
|
Bohler-Uddeholm BÖHLER S400(M7) High Speed Steel Description: High alloyed molybdenum high speed steel with good resistance and high toughness.Applications: Taps, twist drills, reamers, milling tools, broaches tools, cold extrusion dies.Standards:.. |
|||
CTE, linear | 12.5 µm/m-°C @Temperature 600 °C |
6.94 µin/in-°F @Temperature 1110 °F |
|
Bohler-Uddeholm BÖHLER S401(M1) High Speed Steel Description: Molybdenum high speed steel with high toughness and good cutting ability. Applications: Taps, twist drills, reamers, milling tools, broaches toolsStandards: DIN/EN 1.3346 HS2-91, AISI M.. |
|||
CTE, linear | 12.5 µm/m-°C @Temperature 700 °C |
6.94 µin/in-°F @Temperature 1290 °F |
|
Bohler-Uddeholm BÖHLER S401(M1) High Speed Steel Description: Molybdenum high speed steel with high toughness and good cutting ability. Applications: Taps, twist drills, reamers, milling tools, broaches toolsStandards: DIN/EN 1.3346 HS2-91, AISI M.. |
|||
CTE, linear | 12.5 µm/m-°C @Temperature 20.0 - 400 °C |
6.94 µin/in-°F @Temperature 68.0 - 752 °F |
|
Bohler-Uddeholm BÖHLER W302 SUPERIOR® Premium H13 Tool Steel A premium grade H13 hot work tool steel featuring:Very good toughness properties meeting the requirements of NADCA 207-97, and the superior quality levels of NADCA 207-2003Very good heat checking re.. |
|||
CTE, linear | 12.5 µm/m-°C @Temperature 20.0 - 400 °C |
6.94 µin/in-°F @Temperature 68.0 - 752 °F |
|
Bohler-Uddeholm BÖHLER W403 VMR® Hot Work Tool Steel W403 VMR is a modified hot work alloy with an excellent combination of hot tensile properties and toughness. The balanced properties of this grade are not only due to chemistry modification, but to .. |
|||
CTE, linear | 12.5 µm/m-°C @Temperature 21.0 - 427 °C |
6.94 µin/in-°F @Temperature 69.8 - 801 °F |
|
Carpenter Custom 630 (17-Cr-4Ni) Precipitation Hardening Stainless Steel, Condition H 1100 (Heated 593°C) Data provided by Carpenter Technology Corporation.Custom 630 (17Cr-4Ni) is a martensitic precipitation/age-hardening stainless steel offering high strength and hardness along with excellent corrosio.. |
|||
CTE, linear | 12.5 µm/m-°C @Temperature 20.0 - 800 °C |
6.94 µin/in-°F @Temperature 68.0 - 1470 °F |
|
ATI Allegheny Ludlum Stainless Steel Type 439/AL 439HP™ (ASTM XM-8; UNS S43035) Allegheny Ludlum Stainless Steel Type 439, a titanium stabilized, 18 percent chromium alloy, also known as ASTM XM-8 and by the UNS designation S43035, is a ferritic stainless steel designed to resi.. |
|||
CTE, linear | 12.5 µm/m-°C @Temperature 20.0 - 800 °C |
6.94 µin/in-°F @Temperature 68.0 - 1470 °F |
|
ATI Allegheny Ludlum Stainless Steel Type 439/AL 439HP™, 10% cold work (ASTM XM-8; UNS S43035) Allegheny Ludlum Stainless Steel Type 439, a titanium stabilized, 18 percent chromium alloy, also known as ASTM XM-8 and by the UNS designation S43035, is a ferritic stainless steel designed to resi.. |
|||
CTE, linear | 12.5 µm/m-°C @Temperature 20.0 - 800 °C |
6.94 µin/in-°F @Temperature 68.0 - 1470 °F |
|
ATI Allegheny Ludlum Stainless Steel Type 439/AL 439HP™, 30% cold work (ASTM XM-8; UNS S43035) Allegheny Ludlum Stainless Steel Type 439, a titanium stabilized, 18 percent chromium alloy, also known as ASTM XM-8 and by the UNS designation S43035, is a ferritic stainless steel designed to resi.. |
|||
CTE, linear | 12.5 µm/m-°C @Temperature 20.0 - 600 °C |
6.94 µin/in-°F @Temperature 68.0 - 1110 °F |
|
ATI Allegheny Ludlum Martensitic Stainless Steel Type 420, Hardened + 288°C Temper Allegheny Ludlum Type 420 is a hardenable straight-chromium stainless steel which combines superior wear resistance of high carbon alloys with the excellent corrosion resistance of chromium stainles.. |
|||
CTE, linear | 12.5 µm/m-°C @Temperature 20.0 - 200 °C |
6.94 µin/in-°F @Temperature 68.0 - 392 °F |
Quenched and Tempered |
Schmolz + Bickenbach Cryodur® 2767 Cold Work Die Steel Description: High hardenability and toughness, highly suitable for polishing, texturing and EDM machining. We recommend the use of Cryodur® 2767 (ERS) for extreme demandsApplications: Cutlery dies,.. |
|||
CTE, linear | 12.5 µm/m-°C @Temperature 20.0 - 600 °C |
6.94 µin/in-°F @Temperature 68.0 - 1110 °F |
|
ATI Allegheny Ludlum Martensitic Stainless Steel Type 420, Hardened + 204°C Temper Allegheny Ludlum Type 420 is a hardenable straight-chromium stainless steel which combines superior wear resistance of high carbon alloys with the excellent corrosion resistance of chromium stainles.. |
|||
CTE, linear | 12.5 µm/m-°C @Temperature 20.0 - 600 °C |
6.94 µin/in-°F @Temperature 68.0 - 1110 °F |
|
ATI Allegheny Ludlum Martensitic Stainless Steel Type 420, Hardened + 316°C Temper Allegheny Ludlum Type 420 is a hardenable straight-chromium stainless steel which combines superior wear resistance of high carbon alloys with the excellent corrosion resistance of chromium stainles.. |
|||
CTE, linear | 12.5 µm/m-°C @Temperature 20.0 - 600 °C |
6.94 µin/in-°F @Temperature 68.0 - 1110 °F |
|
ATI Allegheny Ludlum Martensitic Stainless Steel Type 420, Hardened + 482°C Temper Allegheny Ludlum Type 420 is a hardenable straight-chromium stainless steel which combines superior wear resistance of high carbon alloys with the excellent corrosion resistance of chromium stainles.. |
|||
CTE, linear | 12.5 µm/m-°C @Temperature 20.0 - 300 °C |
6.94 µin/in-°F @Temperature 68.0 - 572 °F |
|
Industeel CREUSABRO® 8000 High Performance Wear Resistant Steel Description: CREUSABRO® 8000 is a high performance wear resistant steel, exhibiting a wear resistance of 50% higher than that of conventional 500 HB water quenched steel. CREUSABRO® 8000 is using .. |
|||
CTE, linear | 12.5 µm/m-°C @Temperature 20.0 - 200 °C |
6.94 µin/in-°F @Temperature 68.0 - 392 °F |
|
Industeel URANUS® 45N+ 22% Cr Austenitic-Ferritic Duplex Stainless Steel Description: URANUS® 45N+ (UR 45N+) is a nitrogen alloyed austenitic-ferritic Duplex stainless steel (22.05), with a minimum PREN value guaranteed of 36 due to over-alloying in Molybdenum and Chrom.. |