Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
CTE, linear 12.96 µm/m-°C

@Temperature 260 - 788 °C
7.200 µin/in-°F

@Temperature 500 - 1450 °F
Carpenter Micro-Melt® 9 Hardened and Tempered Tool Steel
Micro-Melt® 9 tool steel is a high vanadium tool steel produced using the Carpenter Micro-Melt powder process. This grade possesses wear resistance superior to most other tool steels along with goo..