Thermal Properties Metric English Comments
CTE, linear 216 µm/m-°C

@Temperature 50.0 - 100 °C
120 µin/in-°F

@Temperature 122 - 212 °F
3D Systems Accura® ClearVue™ Free (SL 7870) Stereolithography Plastic
High clarity plastic for a multitude of applicationsFeaturesClear and transparentRigid and toughGreat for headlamps, bottles and transparent assembliesExcellent humidity/moisture resistanceAll infor..