Polymer Property : CTE, linear = 123 µm/m-°C Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
CTE, linear 123 µm/m-°C

@Temperature 100 - 150 °C
68.3 µin/in-°F

@Temperature 212 - 302 °F
Alpha 2
Tra-Con Tra-Bond 546S04 Thixotropic UV/Blue Light Cure Adhesive
TRA-BOND 546S04 is a thixotropic UV/blue light curable adhesive with a secondary heat cure. TRA-BOND 546S04 is ideal for general optics bonding, mounting of lenses, and glob top applications. The ..