Thermal Properties Metric English Comments
CTE, linear 13.17 µm/m-°C

@Temperature 25.0 - 350 °C
7.317 µin/in-°F

@Temperature 77.0 - 662 °F
Carpenter O6 Graphitic Tool Steel (AISI O6)
Carpenter O6 is an oil-hardening tool steel designed for cold work applications. It is designed to have free graphite in the microstructure. This free graphite is responsible for the excellent machi..