Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear | 24.5 - 25.5 µm/m-°C @Temperature 20.0 - 300 °C |
13.6 - 14.2 µin/in-°F @Temperature 68.0 - 572 °F |
|
PEAK Werkstoff DISPAL S693 Aluminum Alloy, AlCu5Ti, Condition T6 High stiffness and elongation at rupture. Property data for Condition T6 (Quench in water at RT).Information provided by PEAK Werkstoff GmbH |
|||
CTE, linear | 24.5 - 25.5 µm/m-°C @Temperature 20.0 - 300 °C |
13.6 - 14.2 µin/in-°F @Temperature 68.0 - 572 °F |
|
PEAK Werkstoff DISPAL S693 Aluminum Alloy, AlCu5Ti, Condition T4 High stiffness and elongation at rupture. Property data for Condition T4 (Quench in water at RT).Information provided by PEAK Werkstoff GmbH |
|||
CTE, linear | 24.5 µm/m-°C @Temperature 20.0 - 200 °C |
13.6 µin/in-°F @Temperature 68.0 - 392 °F |
|
Alcoa MIC-6 Aluminum Mold Alloy MIC-6 is a blend of the most desirable features of many individual metals. The result is a cast aluminum plate that meets the challenge of product accuracy demanded by today’s industry.Because of i.. |