Polymer Property : CTE, linear = 13.66 µm/m-°C Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
CTE, linear 13.66 µm/m-°C

@Temperature 21.0 - 500 °C
7.589 µin/in-°F

@Temperature 69.8 - 932 °F
Latrobe LSS™ S7 Shock-Resisting Tool Steel (ASTM S7)
TLS S7 Shock-Resisting tool steel is an air or oil hardening tool steel that is characterized by very high impact toughness. The combination of strength and high toughness makes S7 tool steel a cand..