Polymer Property : CTE, linear = 13.8 µin/in-°F Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
CTE, linear 24.8 µm/m-°C

@Temperature 80.0 - 130 °C
13.8 µin/in-°F

@Temperature 176 - 266 °F
ramp rate 10°/min.