Polymer Property : CTE, linear = 135.8 µm/m-°C Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
CTE, linear 114.4 - 135.8 µm/m-°C

@Temperature 50.0 - 100 °C
63.56 - 75.44 µin/in-°F

@Temperature 122 - 212 °F
ASTM E831-00
DSM Somos® ProtoGen™ O-XT 18420 Epoxy Resin for Stereolithography, UV Postcure at HOC -2
DescriptionDSM Somos® ProtoGen O-XT 18420 is a liquid, ABS-like, photopolymer that produces accurate parts ideal for general purpose applications. ProtoGen resins are the first SL resins to demons..