Thermal Properties Metric English Comments
CTE, linear 25.3 - 26.0 µm/m-°C

@Temperature -40.0 - 0.000 °C
14.1 - 14.4 µin/in-°F

@Temperature -40.0 - 32.0 °F
ASTM E831-00
DSM Somos® NanoTool™ Resin for Stereolithography, UV Postcure
DescriptionNanoTool produces strong, stiff, high temperature resistant composite parts on conventional stereolithography machines. This third generation of Somos® ProtoComposite materials is heavi..