Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear | 265 µm/m-°C @Temperature 185 - 260 °C |
147 µin/in-°F @Temperature 365 - 500 °F |
Z-Axis Alpha 2; IPC-TM-650.2.4.41 |
Park Electrochemical Nelco® N4000-29 Multifunctional Epoxy The Nelco N4000-29 is an advanced, lead-free, low-CTE, high Tg (185º C by DSC) multifunctional epoxy dielectric substrate. This material has been designed for use not only in standard multilayer PW.. |
|||
CTE, linear | 265 µm/m-°C @Temperature 175 - 260 °C |
147 µin/in-°F @Temperature 347 - 500 °F |
Z-Axis Alpha 2; IPC-TM-650.2.4.41 |
Park Electrochemical Nelco® N4000-11 Multifunctional Epoxy Laminate and Prepreg The Nelco® N4000-11 is a CAF resistant, high Tg (175º C by DSC) multifunctional epoxy dielectric substrate. This material is formulated to provide the PWB manufacturer and OEM with vastly improved.. |