Polymer Property : CTE, linear = 15.94 µm/m-°C Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
CTE, linear 15.94 µm/m-°C

@Temperature 500 °C
8.856 µin/in-°F

@Temperature 932 °F
Special Metals INCOLOY® alloy 890 Ni-Cr-Fe Superalloy
INCOLOY® alloy 890 (UNS N08890) is the latest addition to the INCOLOY alloy family of heat resistant alloys. Alloy 890 joins the existing INCOLOY products in offering high strength along with ex..