Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
CTE, linear 156 µm/m-°C

@Temperature 50.0 - 100 °C
86.7 µin/in-°F

@Temperature 122 - 212 °F
ASTM E831-00
DSM Somos® 14120 Water-resistant resin for stereolithography, White
DescriptionDSM Somos® 14120 is a low viscosity liquid photopolymer that produces strong, tough, water-resistant parts. Parts created with Somos® 14120 have a white, opaque appearance similar to p..
CTE, linear 156 µm/m-°C

@Temperature -60.0 - 50.0 °C
86.7 µin/in-°F

@Temperature -76.0 - 122 °F
DIN 53122
Arkema Group ORGASOL® 2002 D Nat 1 Polyamide 12, Food Contact Approved
Information provided by Arkema Group