Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
CTE, linear 15.5 - 16.5 µm/m-°C

@Temperature 20.0 - 200 °C
8.61 - 9.17 µin/in-°F

@Temperature 68.0 - 392 °F
PEAK Werkstoff DISPAL S220 Aluminum Alloy, AlSi35, Condition F
Excellent properties:abrasive stabilityhigh stiffness (E-modulus)resistance even at high temperaturesgood grindabilityPEAK DISPAL materials allow the manufacturing of pistons for highest operational..
CTE, linear 15.5 - 16.5 µm/m-°C

@Temperature 20.0 - 200 °C
8.61 - 9.17 µin/in-°F

@Temperature 68.0 - 392 °F
PEAK Werkstoff DISPAL S220 Aluminum Alloy, AlSi35, Condition O
Excellent properties:abrasive stabilityhigh stiffness (E-modulus)resistance even at high temperaturesgood grindabilityPEAK DISPAL materials allow the manufacturing of pistons for highest operational..
CTE, linear 15.5 - 16.5 µm/m-°C

@Temperature 20.0 - 200 °C
8.61 - 9.17 µin/in-°F

@Temperature 68.0 - 392 °F
PEAK Werkstoff DISPAL S225 Aluminum Alloy, AlSi35Fe2Ni, Condition F
Excellent properties:abrasive stabilityhigh stiffness (E-modulus)resistance even at high temperaturesgood grindabilityPEAK DISPAL materials allow the manufacturing of pistons for highest operational..