Thermal Properties Metric English Comments
CTE, linear 170 - 189 µm/m-°C

@Temperature 50.0 - 100 °C
94.4 - 105 µin/in-°F

@Temperature 122 - 212 °F
ASTM E831-00
Proto3000 WaterShed® XC 11122 Stereolithography (SLA) Prototyping Polymer
WaterShed XC is a low viscosity liquid photopolymer that produces strong, tough, water-resistant, ABS-like parts. Most importantly parts created with WaterShed 11122 are nearly colorless, and look ..
CTE, linear 170 - 189 µm/m-°C

@Temperature 50.0 - 100 °C
94.4 - 105 µin/in-°F

@Temperature 122 - 212 °F
UV Postcure; ASTM E831-05
DSM Somos® BioClear
Parts created with Somos® BioClear are designed for medical applications that are non-implant and have limited contact with the body such as device prototyping. They are shatter-resistant so they w..
CTE, linear 170 µm/m-°C

@Temperature 50.0 - 100 °C
94.4 µin/in-°F

@Temperature 122 - 212 °F
UV Postcure; ASTM E831-05
DSM Somos® GP Plus 14122
Somos® GP Plus 14122 is a low-viscosity stereolithography resin with an opaque white appearance. This material mirrors production plastics like ABS and PBT, making it an ideal choice for virtually ..
CTE, linear 170 - 189 µm/m-°C

@Temperature 50.0 - 100 °C
94.4 - 105 µin/in-°F

@Temperature 122 - 212 °F
ASTM E831-00
DSM Somos® WaterShed® XC 11122 Water-resistant resin for stereolithography
DescriptionWaterShed XC is a low viscosity liquid photopolymer that produces strong, tough, water-resistant, ABS-like parts. Most importantly parts created with WaterShed 11122 are nearly colorless..
CTE, linear 170 µm/m-°C

@Temperature 50.0 - 160 °C
94.4 µin/in-°F

@Temperature 122 - 320 °F
DIN 53122
Arkema Group ORGASOL® 1002 D Nat 1 Polyamide 6
Information provided by Arkema Group
CTE, linear 170 µm/m-°C

@Temperature 90.0 - 150 °C
94.4 µin/in-°F

@Temperature 194 - 302 °F
T>Tg; ASTM E831-93
3D Systems Accura® 10 Plastic for SLA® Systems