Thermal Properties Metric English Comments
CTE, linear 18.9 µm/m-°C

@Temperature 25.6 - 649 °C
10.5 µin/in-°F

@Temperature 78.0 - 1200 °F
Carlson Nitronic® 50® Austenitic Stainless Steel
General DescriptionNitronic 50 is a nitrogen-strengthened austenitic stainless steel that possesses corrosion resistance superior to 316, 316L, 317 and 317L plus approximately twice the yield streng..
CTE, linear 18.9 µm/m-°C

@Temperature 20.0 - 1000 °C
10.5 µin/in-°F

@Temperature 68.0 - 1830 °F
ATI Allegheny Ludlum 310 Austenitic Stainless Steel
Characteristics: comparable corrosion resistance, superior resistance to oxidation, and the retention of a larger fraction of room temperature strength than common austenitic alloys. Good creep defo..
CTE, linear 18.9 µm/m-°C

@Temperature 20.0 - 1000 °C
10.5 µin/in-°F

@Temperature 68.0 - 1830 °F
ATI Allegheny Ludlum 310H Austenitic Stainless Steel
Characteristics: comparable corrosion resistance, superior resistance to oxidation, and the retention of a larger fraction of room temperature strength than common austenitic alloys. Good creep defo..
CTE, linear 18.9 µm/m-°C

@Temperature 20.0 - 1000 °C
10.5 µin/in-°F

@Temperature 68.0 - 1830 °F
ATI Allegheny Ludlum 310S Austenitic Stainless Steel
Characteristics: comparable corrosion resistance, superior resistance to oxidation, and the retention of a larger fraction of room temperature strength than common austenitic alloys. Good creep defo..
CTE, linear 18.9 µm/m-°C

@Temperature 20.0 - 1000 °C
10.5 µin/in-°F

@Temperature 68.0 - 1830 °F
ATI Allegheny Ludlum 310Si Austenitic Stainless Steel
Characteristics: comparable corrosion resistance, superior resistance to oxidation, and the retention of a larger fraction of room temperature strength than common austenitic alloys. Good creep defo..
CTE, linear 18.9 µm/m-°C

@Temperature 20.0 - 600 °C
10.5 µin/in-°F

@Temperature 68.0 - 1110 °F
ATI Allegheny Ludlum Stainless Steel Type 348 (UNS S34800)
AL 348 is a stabilized stainless steel which offers excellent resistance to intergranular corrosion following exposure to temperatures in the chromium carbide precipitation range from 800° to 1500°..
CTE, linear 18.9 µm/m-°C

@Temperature 20.0 - 600 °C
10.5 µin/in-°F

@Temperature 68.0 - 1110 °F
ATI Allegheny Ludlum Stainless Steel Type 321 (UNS S32100)
AL 321 is a stabilized stainless steel which offers excellent resistance to intergranular corrosion following exposure to temperatures in the chromium carbide precipitation range from 800° to 1500°..
CTE, linear 18.9 µm/m-°C

@Temperature 20.0 - 600 °C
10.5 µin/in-°F

@Temperature 68.0 - 1110 °F
ATI Allegheny Ludlum Stainless Steel Type 347 (UNS S34700)
AL 347 is a stabilized stainless steel which offers excellent resistance to intergranular corrosion following exposure to temperatures in the chromium carbide precipitation range from 800° to 1500°..