Polymer Property : CTE, linear = 190 µin/in-°F Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
CTE, linear 342 µm/m-°C

@Temperature 85.0 - 145 °C
190 µin/in-°F

@Temperature 185 - 293 °F
ASTM E831
Proto3000 Duraform® EX Selective Laser Sintering (SLS®) Prototyping Polymer
Plastic for use with all Sinterstation® Pro and Sinterstation HiQ™ series SLS® systemsDescription: This impact-resistant plastic offers the toughness of injection-molded polypropylene and ABS and..
CTE, linear 342 µm/m-°C

@Temperature 85.0 - 145 °C
190 µin/in-°F

@Temperature 185 - 293 °F
ASTM E831
3D Systems DuraForm® EX Impact-Resistant Plastic for SLS® Systems
This impact-resistant plastic offers the toughness of injection-molded polypropylene and ABS and is suitable for Rapid Manufacturing. For use with all Sinterstation® Pro and Sinterstation HiQ™ ser..
CTE, linear 342 µm/m-°C

@Temperature 85.0 - 145 °C
190 µin/in-°F

@Temperature 185 - 293 °F
ASTM E831
ALM PA 850 Black Nylon 11 SLS Prototyping Polymer
Information provided by Advanced Laser Materials (ALM).
CTE, linear 342 µm/m-°C

@Temperature 85.0 - 145 °C
190 µin/in-°F

@Temperature 185 - 293 °F
ASTM E831
ALM PA 860 White Nylon 11 SLS Prototyping Polymer
Unfilled White PA 11 that is formulated for easy processing across all LS platforms. Tightly controlled particle distribution creates a smooth surface finish and excellent feature detail. Parts prod..