Polymer Property : CTE, linear = 2.46 µin/in-°F Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
CTE, linear 4.43 µm/m-°C

@Temperature 20.0 - 400 °C
2.46 µin/in-°F

@Temperature 68.0 - 752 °F
CMW® 2000 AMS-T-21014 ASTM B777 High Density Machinable Tungsten
Uses: Radiation Shielding, High Mass, Gyro, Ordnance. Machinability is similar to gray iron.Information provided by CMW Inc.