Thermal Properties Metric English Comments
CTE, linear 5.00 µm/m-°C

@Temperature 900 °C
2.78 µin/in-°F

@Temperature 1650 °F
MarkeTech Repton 504 Mullite
Brand 504 features: Max spall resistance.REPTON setter tiles, kiln furniture, and special fixtures are lightweight, ridge, and high strength ceramics that resist distortion and spalling, even when t..
CTE, linear 5.00 µm/m-°C

@Temperature 900 °C
2.78 µin/in-°F

@Temperature 1650 °F
MarkeTech Repton 601 Mullite
Brand 601 features: High porosity-low bulk density.REPTON setter tiles, kiln furniture, and special fixtures are lightweight, ridge, and high strength ceramics that resist distortion and spalling, e..
CTE, linear 5.00 µm/m-°C

@Temperature 900 °C
2.78 µin/in-°F

@Temperature 1650 °F
MarkeTech Repton 632 Mullite
Brand 632 features: Light Weight Setter.REPTON setter tiles, kiln furniture, and special fixtures are lightweight, ridge, and high strength ceramics that resist distortion and spalling, even when th..
CTE, linear 5.00 µm/m-°C

@Temperature 900 °C
2.78 µin/in-°F

@Temperature 1650 °F
MarkeTech Repton 663 Mullite
Brand 663 features: Zirconia.REPTON setter tiles, kiln furniture, and special fixtures are lightweight, ridge, and high strength ceramics that resist distortion and spalling, even when thermal cycle..
CTE, linear 5.00 µm/m-°C

@Temperature 50.0 °C
2.78 µin/in-°F

@Temperature 122 °F
perpendicular to optical axis
MarkeTech Sapphire (Aluminum Oxide - Al2O3) Single Crystal
Data provided by the supplier, MarkeTech International.Sapphire is grown by several methods: Boule form (Czochralski), in plate form, or as tubes, rods and plates. Boules are grown up to 8" diam..
CTE, linear 5.00 µm/m-°C

@Temperature 20.0 - 450 °C
2.78 µin/in-°F

@Temperature 68.0 - 842 °F
H.C. Starck HPM 1850W Tungsten High Density Composite
Description of Product: Tungsten based composite materials are outstanding due to high density and good mechanical properties. The product can be delivered both as semi-finished product for furthe..
CTE, linear 5.00 µm/m-°C

@Temperature 20.0 - 200 °C
2.78 µin/in-°F

@Temperature 68.0 - 392 °F
CeramTec Rubalit® A 1894 Alumina, 94%
Rubalit® A 1894 (94%) was specifically developed in response to electrical and electronic engineering needs. In conjunction with CeramTec's complementary metallization systems, a vacuum-tight bond ..
CTE, linear 5.00 µm/m-°C

@Temperature 0.000 - 100 °C
2.78 µin/in-°F

@Temperature 32.0 - 212 °F
x direction; IPC TM-650 2.4.24
Arlon AD350A PTFE/Woven Fiberglass/Ceramic Filled Composite
Tighter Dielectric Tolerance Low Z-Axis Thermal ExpansionCeramic Filled PTFEHigh Thermal ConductivityLarge Panel SizeBenefits:Higher Consistency of PerformanceSuperior PTH AdhesionHeat Dissipation a..