Polymer Property : CTE, linear = 20.6 µin/in-°F Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
CTE, linear 37.0 µm/m-°C

@Temperature -55.0 - 288 °C
20.6 µin/in-°F

@Temperature -67.0 - 550 °F
Z-Direction; ASTM D3386-94
Rogers Corporation RO4533 Ceramic-Filled, Glass-Reinforced Hydrocarbon Laminate
The RO4500™ Series Cost Performance Antenna Grade Laminates are ceramic-filled, glass-reinforced hydrocarbon based materials that provides the controlled dielectric constant, low loss performance a..