Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear | 23.9 µm/m-°C @Temperature 30.0 - 80.0 °C |
13.3 µin/in-°F @Temperature 86.0 - 176 °F |
ramp rate 10°/min. |
Nihon Superior SN100C Lead-Free Solder Alloy Allows high productivity in soldering processes and cost effective, reliable joints. Attributes include high fluidity, low copper erosion, low drossing, superior wetting and freedom from shrinkage d.. |