CTE, linear 235 µm/m-°C

@Temperature 20.0 °C
131 µin/in-°F

@Temperature 68.0 °F
Cured property; alpha 2
Aptek 2712-A/B Very low stress silicone adhesive
Very low stress silicone adhesive; -110ºC to 260ºC operating range; Low outgassing/space gradeAPTEK 2712-A/B is a two component, white, very soft, thixotropic, electrically insulative, silicone ad..