Polymer Property : CTE, linear = 236 µm/m-°C Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
CTE, linear 218 - 236 µm/m-°C

@Temperature >=44.0 °C
121 - 131 µin/in-°F

@Temperature >=111 °F
UV Postcure, after Tg; ASTM E831-06
DSM Somos® NeXt LV Grey
The second member of the Somos® NeXt family, Somos® NeXt LV Grey delivers the durability and functionality, with a finer resolution of details and faster part processing. This third-generation, hi..