Polymer Property : CTE, linear = 26.0 µm/m-°C Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
CTE, linear 26.0 µm/m-°C

@Temperature -55.0 - 288 °C
14.4 µin/in-°F

@Temperature -67.0 - 550 °F
Z-Direction; ASTM D3386-94
Rogers Corporation RO4835 Hydrocarbon Ceramic Laminate, Improved Oxidation Resistance
Features and Benefits:Significantly improved oxidation resistance compared to typical thermoset microwave materialsDesigned for performance sensitive, high volume applicationsLow loss - Excellent el..
CTE, linear 26.0 µm/m-°C

@Temperature 0.000 - 140 °C
14.4 µin/in-°F

@Temperature 32.0 - 284 °F
Z-Direction; ASTM D3386
Rogers Corporation TMM® TMM6 Ceramic Thermoset Polymer Composite
TMM® Thermoset microwave materials are ceramic thermoset polymer composites designed for high plate-thru-hole reliability stripline and microstrip applications. The electrical and mechanical prope..
CTE, linear 26.0 µm/m-°C

@Temperature 24.0 - 149 °C
14.4 µin/in-°F

@Temperature 75.2 - 300 °F
ASTM E831-93
Saint-Gobain Meldin® 5055 Thermoplastic Bearing Material
General Notes on Meldin 3000/5000 Series Bearing Products:Injection Moldable, High-Performance Bearings. Can withstand environments of high temperature, corrosive, and water.Specific Notes on Meldin..