Thermal Properties Metric English Comments
CTE, linear 52.2 µm/m-°C

@Temperature 73.0 °C
29.0 µin/in-°F

@Temperature 163 °F
TD; ASTM D696
Mitsui AURUM® JGN3030 Polyimide, Glass Fiber Filled  (discontinued **)
AURUM JGN3030 is a high performance thermoplastic polyimide for precision injection molded components and extruded products. A member of the AURUM family of advanced engineering resins, glass fiber ..