Polymer Property : CTE, linear = 3.26 µin/in-°F Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
CTE, linear 5.86 µm/m-°C

@Temperature 25.0 - 100 °C
3.26 µin/in-°F

@Temperature 77.0 - 212 °F
Carpenter Kovar® Alloy (Glass and Ceramic Sealing Alloy)
Data provided by Carpenter Technology Corporation.Kovar® alloy is a vacuum melted, Fe-Ni-Co, low expansion alloy whose chemical composition is controlled within narrow limits to assure precise unif..