Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : CTE, linear = 3.40 µm/m-°C Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
CTE, linear 3.40 µm/m-°C

@Temperature 20.0 °C
1.89 µin/in-°F

@Temperature 68.0 °F
with grain
Pyrotek PT-10 Graphite
PT-10 Graphite offers the highest resistance to oxidation available. Its unique composition gives it the most durable, long lasting, oxidation resistant properties available from treated graphite.A..
CTE, linear 3.40 µm/m-°C

@Temperature 20.0 - 100 °C
1.89 µin/in-°F

@Temperature 68.0 - 212 °F
DIN EN 821-1
CeramTec Rocar® SiG Silicon Carbide, SiSiC
Rocar® is an extremely lightweight silicon carbide ceramic. It permits a reduction in mass forces at high speeds, and is considered for its hardness, excellent resistance to corrosion and sudden ch..