Polymer Property : CTE, linear = 32.9 µin/in-°F Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
CTE, linear 59.2 µm/m-°C

@Temperature 20.0 - 400 °C
32.9 µin/in-°F

@Temperature 68.0 - 752 °F
ASTM E-233
UBE UPIMOL® S High Heat Polyimide Shape
Description: Ube's UPIMOL is an exceptionally heat-resistant polyimide Shape. This product has the same molecular structure as UPILEX, an ultra-high heat-resistant polyimide film developed by Ub..