Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear | 34.2 µm/m-°C @Temperature 26.7 - 204 °C |
19.0 µin/in-°F @Temperature 80.0 - 400 °F |
x-ply; ASTM D696 |
Park Electrochemical Nelcote® F-502 Phenolic Prepreg, 581 Quartz Reinforced Nelcote® F-502 is a MIL-R-9299 phenolic resin system suitable for impregnation on any MIL-C-9084 fabric with a compatible finish. F-502 is used in the manufacture of ablative reinforcements in rock.. |