Thermal Properties Metric English Comments
CTE, linear 4.10 µm/m-°C

@Temperature 20.0 - 300 °C
2.28 µin/in-°F

@Temperature 68.0 - 572 °F
Schott WG295 Long Pass Filter
Base glass. Data provided by the manufacturer, Schott Glas Mainz.Similar glasses include GG395, GG400, GG420, GG435, GG455, GG475, GG495, OG515, OG530, OG550, OG570, OG590, RG610, RG630, RG645, RG66..
CTE, linear 4.10 µm/m-°C

@Temperature 20.0 - 600 °C
2.28 µin/in-°F

@Temperature 68.0 - 1110 °F
DIN EN 821-1
CeramTec Rocar® S Silicon Carbide, SSiC
Rocar® is an extremely lightweight silicon carbide ceramic. It permits a reduction in mass forces at high speeds, and is considered for its hardness, excellent resistance to corrosion and sudden ch..
CTE, linear 4.10 µm/m-°C

@Temperature 20.0 - 400 °C
2.28 µin/in-°F

@Temperature 68.0 - 752 °F
DIN EN 821-1
CeramTec Rocar® SiG Silicon Carbide, SiSiC
Rocar® is an extremely lightweight silicon carbide ceramic. It permits a reduction in mass forces at high speeds, and is considered for its hardness, excellent resistance to corrosion and sudden ch..