Thermal Properties Metric English Comments
CTE, linear 43.0 µm/m-°C

@Temperature 50.0 - 200 °C
23.9 µin/in-°F

@Temperature 122 - 392 °F
DIN 53 752
Ensinger TECASINT 1011 Polyimide (PI)
TECASINT is a range of non-melting high temperature polyimides characterized by high strength over a wide range of temperatures, good long term thermal stability, minimal thermal expansion and excel..
CTE, linear 43.0 µm/m-°C

@Temperature -30.0 - 0.000 °C
23.9 µin/in-°F

@Temperature -22.0 - 32.0 °F
100 x 15 x 3 mm sample; AZDEL Test
Azdel Plus R300B01N 30% Continuous Random Fiber Mat / PP Resin Matrix
AZDEL® R300B01N is a random oriented needled continuous glass fiber mat material. This polypropylene composite material features high properties and a homogeneous fiber distribution. This materia..
CTE, linear 43.0 µm/m-°C

@Temperature -30.0 - 0.000 °C
23.9 µin/in-°F

@Temperature -22.0 - 32.0 °F
100 x 15 x 3 mm sample; AZDEL Test
Azdel Plus R401B02N 40% Continuous Random Fiber Mat / PP Resin Matrix
AZDEL® R401B02N is a random oriented needled continuous glass fiber mat material. This polypropylene composite material features high properties and a basic homogeneous fiber distribution. This m..
CTE, linear 43.0 µm/m-°C

@Temperature -30.0 - 0.000 °C
23.9 µin/in-°F

@Temperature -22.0 - 32.0 °F
100 x 15 x 3 mm sample; AZDEL Test
Azdel Plus R301B01N 30% Continuous Random Fiber Mat / PP Resin Matrix
AZDEL® R301B01N is a random oriented needled continuous glass fiber mat material. This polypropylene composite material features high properties and a basic homogeneous fiber distribution. This m..