Polymer Property : CTE, linear = 44.8 µin/in-°F Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
CTE, linear 80.7 µm/m-°C

@Temperature 0.000 - 50.0 °C
44.8 µin/in-°F

@Temperature 32.0 - 122 °F
ASTM E831-00
DSM Somos® ProtoTherm™ 12120 Water-resistant resin for stereolithography, UV Postcure
DescriptionDSM Somos® 12120 is a liquid photopolymer that produces strong, high temperature tolerant, water-resistant parts. Parts created with Somos® 12120 have a cherry-red appearance which tur..