Polymer Property : CTE, linear = 5.02 µin/in-°F Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
CTE, linear 9.03 µm/m-°C

@Temperature 20.0 - 1000 °C
5.02 µin/in-°F

@Temperature 68.0 - 1830 °F
parallel to c-axis
MarkeTech Sapphire (Aluminum Oxide - Al2O3) Single Crystal
Data provided by the supplier, MarkeTech International.Sapphire is grown by several methods: Boule form (Czochralski), in plate form, or as tubes, rods and plates. Boules are grown up to 8" diam..