Thermal Properties Metric English Comments
CTE, linear 5.30 µm/m-°C

@Temperature 20.0 - 450 °C
2.94 µin/in-°F

@Temperature 68.0 - 842 °F
H.C. Starck HPM 1705 Tungsten High Density Composite
Description of Product: Tungsten based composite materials are outstanding due to high density and good mechanical properties. The product can be delivered both as semi-finished product for furthe..
CTE, linear 5.30 µm/m-°C

@Temperature 20.0 - 300 °C
2.94 µin/in-°F

@Temperature 68.0 - 572 °F
H.C. Starck HPM 1810 Tungsten High Density Composite
Description of Product: Tungsten based composite materials are outstanding due to high density and good mechanical properties. The product can be delivered both as semi-finished product for furthe..
CTE, linear 5.30 µm/m-°C

@Temperature -30.0 - 70.0 °C
2.94 µin/in-°F

@Temperature -22.0 - 158 °F
Schott KG3 Short Pass Filter
Ionically colored glass. Data provided by the manufacturer, Schott Glas Mainz.Similar glasses include KG2, KG1, KG4, KG5
CTE, linear 5.30 µm/m-°C

@Temperature -30.0 - 70.0 °C
2.94 µin/in-°F

@Temperature -22.0 - 158 °F
Schott LAFN7 Glass
Information Provided by SCHOTT North America, Inc.
CTE, linear 5.30 µm/m-°C

@Temperature 20.0 - 100 °C
2.94 µin/in-°F

@Temperature 68.0 - 212 °F
Special Metals NILO® Alloy 42 Controlled-Expansion Alloy
Inflection point 370°C. A nickel-iron controlled-expansion alloy containing 42% nickel. It has a low and nominally constant coefficient of thermal expansion from room temperature to about 570Â..
CTE, linear 5.30 µm/m-°C

@Temperature -30.0 - 70.0 °C
2.94 µin/in-°F

@Temperature -22.0 - 158 °F
Schott KG1 Short Pass Filter
Ionically colored glass. Data provided by the manufacturer, Schott Glas Mainz.Similar glasses include KG2, KG3, KG4, KG5
CTE, linear 5.30 µm/m-°C

@Temperature -30.0 - 70.0 °C
2.94 µin/in-°F

@Temperature -22.0 - 158 °F
Schott N-LAF35 Glass
Information Provided by SCHOTT North America, Inc.
CTE, linear 5.30 µm/m-°C

@Temperature 20.0 - 300 °C
2.94 µin/in-°F

@Temperature 68.0 - 572 °F
ASTM-C372
CeramTec Rubalit® 600 Alumina, 48%
Rubalit® 600 is suitable for both mechanical and laser trimming and is chiefly used as the core for high-grade carbon-film resistors.
CTE, linear 5.30 µm/m-°C

@Temperature 25.0 - 800 °C
2.94 µin/in-°F

@Temperature 77.0 - 1470 °F
CoorsTek ACI-Co6 Tungsten Carbide
Applications: seal rings, plungers, liners, nozzles, valve components, pump components, wear components in the oil & gas, construction, and agriculture equipment industries
CTE, linear 5.30 µm/m-°C

@Temperature 30.0 - 450 °C
2.94 µin/in-°F

@Temperature 86.0 - 842 °F
Carpenter Kovar® Alloy (Glass and Ceramic Sealing Alloy)
Data provided by Carpenter Technology Corporation.Kovar® alloy is a vacuum melted, Fe-Ni-Co, low expansion alloy whose chemical composition is controlled within narrow limits to assure precise unif..