CTE, linear 5.36 µm/m-°C

@Temperature 20.0 - 800 °C
2.98 µin/in-°F

@Temperature 68.0 - 1470 °F
CMW® 3000 AMS-T-21014 AMS-7725 High Density Machinable Tungsten
Uses: Radiation Shielding, High Mass, Gyro, Ordnance. Machinability is similar to gray iron.Information provided by CMW Inc.