Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear | 10.6 µm/m-°C @Temperature 21.1 - 260 °C |
5.90 µin/in-°F @Temperature 70.0 - 500 °F |
|
Crucible Steel 422 Stainless Steel Crucible 422 is a hardenable martensitic stainless steel which is being widely used for high temperatures up to 1200°F. It has excellent creep-rupture properties in the range of 600/1200°F and is.. |
|||
CTE, linear | 10.6 µm/m-°C @Temperature 399 °C |
5.90 µin/in-°F @Temperature 750 °F |
hardened and tempered |
Bohler-Uddeholm UDDEHOLM VANADIS 60 Powder Metallurgically Produced Tool Steel Uddeholm Vanadis 60 is a high alloyed powder metallurgical high speed steel suitable for very demanding cold work applications and for cutting tools. The high carbon and alloying content, Co, Mo, W .. |
|||
CTE, linear | 10.6 µm/m-°C @Temperature 21.1 - 93.3 °C |
5.90 µin/in-°F @Temperature 70.0 - 200 °F |
|
Schmolz + Bickenbach Formadur® PH X Superclean Plastic Mold Steel Description: Formadur® PH X Superclean is a corrosion-resistant, martensitic precipitation hardened stainless steelCharacteristics: Excellent resistance to corrosion; Excellent polishability; Excel.. |
|||
CTE, linear | 10.6 µm/m-°C @Temperature 21.1 - 204 °C |
5.90 µin/in-°F @Temperature 70.0 - 400 °F |
|
Schmolz + Bickenbach CorroPlast® Plastic Mold Steel Description: CorroPlast® is a pre-hardened, free-machining 400 series stainless steel, specifically developed for mold bases for processing plastic; and Supplied in the pre-hardened condition with .. |