Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear | 99.0 µm/m-°C @Temperature >=79.0 °C |
55.0 µin/in-°F @Temperature >=174 °F |
above Tg |
Resinlab® EP1285HD-9 Highly Filled, Medium Viscosity Casting Resin Resinlab™ EP1285 (Formerly Lab Product W021901 series) is a highly filled, medium viscosity black casting resin designed for applications requiring a high degree of thermal conductivity and a low C.. |
|||
CTE, linear | 99.0 µm/m-°C @Temperature 20.0 °C |
55.0 µin/in-°F @Temperature 68.0 °F |
Cured property; alpha 1; Perkin Elmer TMS-2 |
Aptek 6109-A/B Epoxy Encapsulant Optoelectronic grade flexible water clear encapsulant. Higher viscosity/lower Tg version for clear blob-top encapsulation of ceramic substrate devicesPart A is blue. Part B is clear to pale yellow.I.. |