Polymer Property : CTE, linear = 56.0 µm/m-°C Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
CTE, linear 56.0 µm/m-°C

@Temperature 200 - 300 °C
31.1 µin/in-°F

@Temperature 392 - 572 °F
DIN 53 752
Ensinger TECASINT 4201 SD Polyimide, Black, Carbon Fiber (PI)
TECASINT is a range of non-melting high temperature polyimides characterized by high strength over a wide range of temperatures, good long term thermal stability, minimal thermal expansion and excel..